Research Article

Template-Free Electrochemical Preparation of Hexagonal CuSn Prism-Structural Electrode for Lithium-Ion Batteries

Figure 3

SEM images (a, b, and c) and XRD patterns (d) of the as-deposited Cu-Sn in electrolyte with 0.06 mol L−1 CuCl and 0.03 mol L−1 SnCl2 at a current density of 0.04 A cm−2 for different deposition times: (A) 0.5 h, (B) 1 h, and (C) 1.5 h.
(a)
(b)
(c)
(d)