Research Article

Stretchable and Hydrophobic Electrochromic Devices Using Wrinkled Graphene and PEDOT:PSS

Figure 3

(a) Photographs of the flexible electrochromic device (ECD) in reduced (blue) and oxidized (bleached) states while it is being flexed under applied voltage of ±15 V, showing a steady color change. (b) Change in transmittance percentage with variable uniaxial strains of , , and . The reduction transparency of the device increases with applied strains with a net transparency of 41.48% at to 46.81% at . A simultaneous decrease in transmittance is observed at the oxidized state with 61.84% transmittance at to 55.72% transmittance at . The schematic (right) depicts the method of applied strain on the device.
(a)
(b)