Research Article

Graphene Synthesis Using a CVD Reactor and a Discontinuous Feed of Gas Precursor at Atmospheric Pressure

Figure 6

Raman spectra for (a) graphene synthesized at different temperatures with a fixed C2H2 flowrate (100 sccm) and (b) with different C2H2 flow rates at 1000°C. Schematic representation for and ratios at (c) fixed flow rate and (d) fixed temperature.
(a)
(b)
(c)
(d)