Research Article

Piezoelectric and Dielectric Characterization of MWCNT-Based Nanocomposite Flexible Films

Figure 7

SEM micrograph images of the dispersion of MWCNTs that have been ultrasonicated in ethanol for 4 hours at (a) MWCNT = 36.4 mg (MWCNT 1), (b) MWCNT = 72.9 mg (MWCNT 2), and (c) MWCNT = 109.35 (MWCNT 3) show smaller agglomerations of MWCNT clusters.
(a)
(b)
(c)