Research Article
A Simple and Reliable Synthesis of Superparamagnetic Magnetite Nanoparticles by Thermal Decomposition of Fe(acac)3
Table 1
Experimental
values and lattice spacing of MNP-I and MNP-II; Standard lattice spacing and corresponding plane assignation of Fe
3O
4.
| MNP-I | 2θ (°) | 17.6 | 30.0 | 35.4 | 37.0 | 43.2 | 53.7 | 57.1 | 62.6 | 71.2 | 73.9 | 79.3 | (Å) | 5.04 | 2.98 | 2.54 | 2.43 | 2.09 | 1.72 | 1.61 | 1.48 | 1.32 | 1.28 | 1.21 | MNP-II | 2θ (°) | 18.3 | 30.2 | 35.5 | 37.1 | 43.2 | 53.5 | 57.1 | 62.7 | 71.1 | 74.2 | 79.2 | (Å) | 4.84 | 2.96 | 2.52 | 2.42 | 2.09 | 1.71 | 1.61 | 1.48 | 1.32 | 1.28 | 1.21 | Standard values | Fe3O4 | 4.86 | 2.98 | 2.53 | 2.43 | 2.10 | 1.71 | 1.62 | 1.48 | 1.33 | 1.28 | 1.21 | | 111 | 220 | 311 | 222 | 400 | 422 | 511 | 440 | 620 | 533 | 444 |
|
|