Research Article

Determination of Electrospinning Parameters’ Strength in Poly(D,L)-lactide-co-glycolide Micro/Nanofiber Diameter Tailoring

Figure 4

SEM image and fiber diameter distribution of electrospun micro/nanofibers using the optimum processing condition (the use of HFIP as the solvent, a PLGA concentration of 30%, a flow rate of 0.6 mL/h, a voltage of 15 kV, and a nozzle-collector distance of 8 cm).