Research Article
Determination of Electrospinning Parameters’ Strength in Poly(D,L)-lactide-co-glycolide Micro/Nanofiber Diameter Tailoring
Table 2
L’18 (35) orthogonal array utilized in the experiments.
| Exp | A | B | C | D | E | (nm) | (nm) | S/N (dB) |
| 1 | 1 | 1 | 1 | 1 | 1 | 1129.8 | 648.4 | -62.2 | 2 | 2 | 2 | 2 | 2 | 2 | 3689.5 | 2424.6 | -72.8 | 3 | 3 | 3 | 3 | 3 | 3 | 4774.0 | 2292.8 | -74.4 | 4 | 1 | 1 | 2 | 2 | 3 | 1414.6 | 949.6 | -64.6 | 5 | 2 | 2 | 3 | 3 | 1 | 2165.0 | 637.0 | -67.0 | 6 | 3 | 3 | 1 | 1 | 2 | 1746.0 | 1079.4 | -66.2 | 7 | 1 | 2 | 1 | 3 | 2 | 24594.4 | 5061.7 | -87.9 | 8 | 2 | 3 | 2 | 1 | 3 | 3437.5 | 2135.5 | -72.1 | 9 | 3 | 1 | 3 | 2 | 1 | 2298.1 | 780.9 | -67.7 | 10 | 1 | 3 | 3 | 2 | 2 | 4121.6 | 2462.6 | -73.6 | 11 | 2 | 1 | 1 | 3 | 3 | 2091.6 | 1535.7 | -68.2 | 12 | 3 | 2 | 2 | 1 | 1 | 980.8 | 492.1 | -60.8 | 13 | 1 | 3 | 3 | 1 | 3 | 1861.6 | 2437.1 | -69.7 | 14 | 2 | 1 | 1 | 2 | 1 | 1869.3 | 592.5 | -65.8 | 15 | 3 | 2 | 2 | 3 | 2 | 4207.6 | 4966.0 | -76.2 | 16 | 1 | 2 | 2 | 3 | 1 | 1189.8 | 638.6 | -62.6 | 17 | 2 | 3 | 3 | 1 | 2 | 1753.8 | 848.8 | -65.7 | 18 | 3 | 1 | 1 | 2 | 3 | 1938.2 | 768.2 | -66.3 |
|
|