Research Article
Electrochemical Epitaxial Growth of TiO2/CdS/PbS Nanocables
Table 2
Photovoltage characteristics of photoanodes.
| Sample | Photocurrent density (mA cm-2) | Output potential difference vs. Ag/AgCl (V) | Fill factor |
| CdS 10 min | 2.04 | 0.98 | 0.57 | CdS 20 min | 2.17 | 1.03 | 0.62 | CdS 30 min | 1.92 | 0.92 | 0.42 | PbS 10 min | 3.36 | 0.90 | 0.26 | CdS 10 min + PbS 10 min | 7.83 | 0.94 | 0.63 |
|
|