Research Article

Enhancing Biocompatibility without Compromising Material Properties: An Optimised NaOH Treatment for Electrospun Polycaprolactone Fibres

Figure 5

Quantification of protein deposition on NaOH-treated (1 M 4 h) and untreated (0 M 0 h) electrospun PCL fibres with random (R) and aligned (A) orientations. Data are shown as deviation with one-way ANOVA and Tukey’s multiple comparisons test (; ).