Synthesis of MWCNT Forests with Alumina-Supported Fe2O3 Catalyst by Using a Floating Catalyst Chemical Vapor Deposition Technique

Figure 10

TEM micrographs of MWCNT bundles synthesized at different CVD temperatures by using the 0.3 g catalyst.
(a) CNTs grown at a CVD temperature of 600°C
(b) CNTs grown at a CVD temperature of 700°C
(c) CNTs grown at a CVD temperature of 800°C
(d) CNTs grown at a CVD temperature of 900°C
(e) CNTs grown at a CVD temperature of 1000°C