Influence of Bath Temperature and Deposition Time on Topographical and Optical Properties of Nanoparticles ZnS Thin Films Synthesized by a Chemical Bath Deposition Method
Figure 6
AFM images for ZnS thin films/glass at different bath temperatures: for deposition time of 30 min.