Research Article

Influence of Bath Temperature and Deposition Time on Topographical and Optical Properties of Nanoparticles ZnS Thin Films Synthesized by a Chemical Bath Deposition Method

Table 4

The values of energy gap , single oscillator energy (), dispersion energy (), and refractive index () for the ZnS films deposited at different times: 20, 30, 40, and 50 min.

Deposition times (min) (eV) (eV) (eV)

204.054.06 (≈)1.231.14
304.015.53 (=1.37 )2.251.18
403.995.6 (=1.4 )4.481.34
503.975.7 (=1.44 )8.761.59