Research Article

Use of Pluronic P103 Triblock Copolymer as Structural Agent during Synthesis of Hybrid Silver Nanoparticles

Table 1

Size distribution of Ag-NPs synthesized at different Pluronic P103 concentrations, at 25°C.

Concentration of Pluronic P103 (wt%)Size (nm) (intensity)Size (nm) (number)Size (nm) (volume)

03.1; 11.7; 76.32.72.6
0.0118, 120911
0.15
0.551
1239