Research Article

Synthesis, Characterization, and Photocatalytic Activity of ZnO Nanomaterials Prepared by a Green, Nonchemical Route

Table 3

BET surface areas of ZnO nanoparticles thermally decomposed at 450, 550, 650, and 750°C.

Sample (m2/g)a

ZnO-4506.8
ZnO-5504.8
ZnO-6503.3
ZnO-7502.4

aBET surface area calculated from the linear part of the BET plot.