Efficacy of Gold Photothermal-Activated Shape Memory Polyurethane
Figure 2
Prepared gold nanorods: TEM (a) of purified rods with an aspect ratio of ~3.25 and a diameter of ~11.5 nm; UV-vis absorption spectra (b) of purified rods showing a longitudinal absorption peak centered at ~830 nm.