Research Article

Preparation of Sol-Enhanced Ni–P–Al2O3 Nanocomposite Coating by Electrodeposition

Table 2

Compositions of bath solution.

Bath compositionsConcentration (g·L-1)Depositing parametersValues

NiSO4•6H2O230Temperature (°C)45, 50, 55, 60
H3BO330pH3.5, 4, 4.5, 5
NaH2PO2•H2O15Current density (A/dm2)0.5, 1, 1.5, 2
NiCl2•6H2O15Time (min)10
Al2O3 sol wt20% (60-70 nm)80 ml/L
C12H25SO4Na0.4