Research Article

Study on the Synergies of Nanoclay and MWCNTs to the Flame Retardant and Mechanical Properties of Epoxy Nanocomposites

Figure 3

FE-SEM image of the fractured surface dragging the nanocomposite materials MWCNTs/epoxy E 240: (a) ultrasonic vibration for 6 hours; (b) stirring mechanically for 7 hours, ultrasonic vibration for 6 hours; (c) stirring mechanically for 8 hours, ultrasonic vibration for 6 hours; (d) stirring mechanically for 9 hours, vibrating ultrasound for 6 hours.
(a)
(b)
(c)
(d)