Research Article
The Role of Tetra Hybrid Reinforcements on the Behavior of Aluminum Metal Matrix Composites
Table 6
Powder metallurgical process parameters for this study [
38].
| Samples | Chemical composition | PM processing parameters |
| Pure Al | Al | (1) Milling time = 2 hrs. (2) Compacting pressure = 60 MPa (3) Sintering temperature = 550°C (4) Sintering time = 3 hrs. | AS1 | Al/5SiC/5Al2O3 | AS2 | Al/5SiC/5Al2O3/0.5Gr/0.5SCBA | AS3 | Al/5SiC/5Al2O3/2.5Gr/2.5SCBA | AS4 | Al/5SiC/5Al2O3/4.5Gr/4.5SCBA | AS5 | Al/5SiC/5Al2O3/6.5Gr/6.5SCBA |
|
|