Optimization on Powder Metallurgy Process Parameters on Nano Boron Carbide and Micron Titanium Carbide Particles Reinforced AA 4015 Composites by Taguchi Technique

Table 2

Composite development based on a plausible combination of process criterion.

Exp no.123456789

Sintering time (hour)2222.252.252.252.52.52.5
Sintering temperature (°C)620640660620640660620640660
Compaction pressure (MPa)300350400350400300400300350