Research Article
Investigation on Hot Corrosion Behaviour of Inconel 625 and Incoloy 800H Superalloys with YSZ-Thermal Barrier Coating Under High-Temperature Environment for Bioreactor Applications
Figure 16
SEM images of Inconel 625 specimens. (a) Uncoated 8-hour-heated 300x magnification. (b) Uncoated 12-hour-heated 300x magnification. (c) Uncoated 16-hour-heated 300x magnification. (d) Uncoated 8-hour-heated 300x magnification. (e) Uncoated 12-hour-heated 300x magnification. (f) Uncoated 16-hour-heated 300x magnification.
(a) |
(b) |
(c) |
(d) |
(e) |
(f) |