Results of wear experiments with a S/N ratio.
| Exp. No. | Wear (μm) | S/N ratio |
| 1 | 63.08 | -37.06 | 2 | 82.14 | -39.39 | 3 | 86.38 | -39.84 | 4 | 78.4 | -38.99 | 5 | 86.69 | -39.87 | 6 | 90.92 | -40.29 | 7 | 86.48 | -39.85 | 8 | 92.17 | -40.41 | 9 | 115.01 | -42.36 | 10 | 49.99 | -35.00 | 11 | 67.41 | -37.65 | 12 | 80.02 | -39.17 | 13 | 69.96 | -37.98 | 14 | 80.18 | -39.19 | 15 | 87.00 | -39.91 | 16 | 74.56 | -38.54 | 17 | 86.68 | -39.87 | 18 | 97.13 | -40.88 | 19 | 37.54 | -32.44 | 20 | 48.43 | -34.72 | 21 | 67.54 | -37.67 | 22 | 44.08 | -33.88 | 23 | 58.8 | -36.44 | 24 | 71.84 | -38.22 | 25 | 56.85 | -36.14 | 26 | 71.57 | -38.18 | 27 | 80.29 | -39.20 |
|
|