Research Article
Effect of Alloying Elements and Ceramic Coating on the Surface Temperature of an Aluminum Piston in a Diesel Engine
Table 2
Thermal boundary condition parameters for pistons with various alloying elements [
10].
| Position | | Temperature (°C) | Film coefficient (W/m2°C) |
| Piston crown | Outer | 1140 | 489 | Central | 1140 | 578 | Interior loop | 1150 | 675 | Upper peripheral surface | 1150 | 751 | Lower peripheral surface | 1150 | 765 | Bottom | 1150 | 486 |
| Combustion chamber | Below the center | 1150 | 395 | Above the center | 1150 | 239 | Central top | 1150 | 202 | Center | 1150 | 328 |
| Firepower shore | | 200 | 163 |
| First ring groove | Upper surface | 180 | 2260 | Bottom | 180 | 2120 | Below surface | 180 | 2223 |
| First ring shore | | 180 | 470 |
| Second ring groove | Upper surface | 170 | 2080 | Bottom | 170 | 1911 | Below surface | 170 | 1972 |
| Second ring shore | | 170 | 432 |
| Third ring groove | Upper surface | 150 | 1961 | Bottom | 150 | 1909 | Below surface | 150 | 2036 |
| Third ring shore | | 150 | 325 |
| Piston skirt | | 150 | 487 |
| Oil return hole | | 150 | 778 |
| Pin hole | | 140 | 324 |
| Inner cavity | Upper surface | 130 | 613 | Upper peripheral surface | 100 | 435 | Middle peripheral surface | 130 | 396 | Lower peripheral surface | 130 | 335 |
|
|