Effect of Temperature Sintering on Grain Growth and Optical Properties of TiO2 Nanoparticles

Table 1

Anatase and rutile phase compositions and crystallite size of TiO2 nanoparticles sintered at 500–900°C for 1 hr.

Calcined temperature (°C)Crystal phase (%)Crystallite size (nm)
AnataseRutileAnataseRutile

50010023
60078223138
70014863442
80010049
90010062