Research Letter

Growth of Functional FeTi Clusters Covered with Carbon Layer

Figure 4

HRTEM image of FeTi particles produced in H 2 gas atmosphere. Particles were covered by a graphitic carbon layer as indicated by arrows. The left top enlarged image of (110) FeTi shows the Guinier-Preston zone-like contrast [8]. This suggests that hydrogen atoms are dissolved in the FeTi crystal.
734940.fig.004