Research Article

Light-Emitting Polymer Nanocomposites

Table 3

Agglomerate diameters and complex viscosity percent difference of ligand capped nanocrystals in PMMA.

LigandLigand to nanoparticle ratioDiameter (nm)Complex viscosity percent difference

ASA2 : 1252 ± 6681%
3 : 1420 11666%
4 : 1349 ± 8558%
5 : 1233 ± 4168%

PA2 : 1444 13844%
3 : 1150 10582%
4 : 1457 ± 17653%
5 : 1242 ± 2470%