Effect of the Thickness of Insulator Polymeric Films on the Memory Behavior: The Case of the Polymethylmethacrylate and the Polystyrene

Figure 6

I-V response of an Al/PMMA (22 nm)/Al memory device. In addition to the threshold voltage at 2 V, threshold voltages at −12 and 20 V are observed.