Large-Scale Atmospheric Step-and-Repeat UV Nanoimprinting

Figure 4

Bubble defects: (a) in the case of low-viscosity resin, bubble defects were observed, and (b) in case of high-viscosity resin, bubble defects were not observed.
103439.fig.004a
(a)
103439.fig.004b
(b)