CNF growth in 10% H2 (2% C2H2, 88% N2). Temperature: (a) 420°C, (b) 470°C, (c) 520°C, (d) 570°C, (e) 670°C, and (f) 770°C. Sample faceted at 815°C (Table 1 (Phase 2)).