Cyclosporine A Loaded PLGA Nanoparticles for Dry Eye Disease: In Vitro Characterization Studies

Table 4

Particle size, PDI of CsA loaded NPs after and before freeze drying (FD) and production yield of NPs.

NPs codeParticle size before FD (nm)Polydispersity index (PDI) before FDParticle size after FD (nm)Polydispersity index (PDI) after FDProduction yeild

F1160.0 ± 08 161.20 ± 100.640 ± 0.05352.29 ± 2.4
F2182.98 ± 130.265 ± 0.084204.30 ± 120.460 ± 0.08155.72 ± 3.1
F3130.5 ± 100.105 ± 0.042145.5 ± 120.262 ± 0.05485.30 ± 2.1
F4128.48 ± 130.388 ± 0.060145.7 ± 130.582 ± 0.06564.90 ± 3.0
F5144.53 ± 130.208 ± 0.045170.5 ± 14.50.508 ± 0.05180.45 ± 2.6
F6210.75 ± 160.458 ± 0.043226.3 ± 180.655 ± 0.04881.90 ± 1.9
F7235.2 ± 19.50.198 ± 0.058244.1 ± 230.669 ± 0.06356.87 ± 2.8
F8240.68 ± 220.410 ± 0.063258.3 ± 24.50.620 ± 0.05880.39 ± 2.5
F9253.50 ± 180.404 ± 0.057260.0 ± 260.474 ± 0.06683.40 ± 2.8

Data as mean SD, , *FD: Freeze drying.