Research Article
Synthesis of Graphene-Based Nanocomposite and Investigations of Its Thermal and Electrical Properties
Table 1
FTIR dip positions and their origin for PMNA and GE-CH-PMNA.
| Chemical | Peak position (cm−1) | Assignment |
| PMNA | 3656 | OH stretching | 3402 | OH stretching | 3205 | –O–H stretch | 2723 | C–H medium | 2267 | Alkynes stretch | 1678 | Alkenes stretch | 1513 | Benzene and quinoid ring | 1295 | Amine stretch | 1112 | C–N medium | 802 | Alkyl halide stretch | 741 | C–Cl stretch |
| GE-CH-PMNA | 3751 | –OH stretching | 3434 | –OH stretching | 2971 | –O–H stretch | 2883 | –CH2 | 1775 | C=O stretching arising from carbonyl and carboxylic groups | 1664 | C=N medium | 1585 | PMNA ring vibration | 1410 | PMNA ring vibration | 1245 | C–O strong | 1175 | N–C stretching | 1098 | C–O stretch | 751 | =C–H bending |
|
|