Research Article

Structure and Electrochemical Properties of a Mechanochemically Processed Silicon and Oxide-Based Nanoscale Composite as an Active Material for Lithium-Ion Batteries

Table 1

Amounts of Si, H2O, and Cu used in the grinding process.

Si : O = 10 : 00.330.50.7511.31.53

Si (g)2.01.951.941.911.881.841.821.68
H2O (g)00.050.060.090.120.160.180.32
Cu (g)0.280.280.280.280.280.280.280.28