Research Article

Controlling the Structure of Hydroxyapatite Ceramics with Dual Pores Prepared Using Freeze-Casting

Table 1

The content of H2O2 in the ceramic slurry before and after milling.

% H2O2 (v/v)The content of H2O2 before milling (ml)The content of H2O2 after milling (ml)The content of decomposed H2O2 during milling (ml)

36.754.132.62
922.515.197.31