Low-Temperature Synthesis of Vanadium Dioxide Thin Films by Sol-Gel Dip Coating Method

Figure 1

XRD patterns of the vanadium oxide thin films prepared at various conditions: (a) T = RT, 400, 450, and 500°C (P = 2 × 10−2 mbar, 1-step calcination), (b) P = 2 × 10−2 and 2 × 10−3 mbar (T = 500°C, 1-step calcination), and (c) 1- and 2-step calcination (P = 2 × 10−3 mbar, T = 500°C).
(a)
(b)
(c)