Review Article

Fiber Optic Chemical Nanosensors Based on Engineered Single-Walled Carbon Nanotubes

Figure 14

Response and recovery times obtained by exposing the sensor SOF-4 to (a) toluene and (b) xylene vapors, at room temperature.
936074.fig.014a
(a)
936074.fig.014b
(b)