Fiber Optic Chemical Nanosensors Based on Engineered Single-Walled
Carbon Nanotubes
Figure 28
Mean response and recovery times obtained exposing the optochemical
sensor coated by 20 monolayers of CdA/SWCNT nanocomposite (75 wt.%) to toluene
and xylene vapors, at room temperature.