Review Article

Fiber Optic Chemical Nanosensors Based on Engineered Single-Walled Carbon Nanotubes

Figure 29

Time responses of the optochemical sensor coated by 20 monolayers of CdA/SWCNT nanocomposite (75 wt.%), exposed to different concentrations of toluene in water at room temperature.
936074.fig.029