Response, response time, and recovery time of Pd-Ag/ZnO Schottky sensor with different concentrations of CH4 in nitrogen using unmodified and Pd modified ZnO thin films at the corresponding optimum temperatures and voltages (calculated from Figures 6(b) and 9(a)).

% of CH4ResponseResponse time (s)Recovery time (s)
ZnOPd: ZnOZnOPd: ZnOZnOPd: ZnO


0.010.9918.222.310.248.318.7
0.051.3822.319.76.746.217.2
0.12.2123.216.46.0338.116.8
0.53.1125.212.14.0220.216.1
13.8132.28.82.691616.0