Electrophoretic Deposition of SnO2 Nanoparticles and Its LPG Sensing Characteristics
Figure 7
SEM images of unsintered SnO2 (a), sintered SnO2 at 300°C-400-500-600°C for 5 minutes (b–e), and side view of film thickness (f).
(a) Unsintered |
(b) 300°C |
(c) 400°C |
(d) 500°C |
(e) 600°C |
(f) Side view of SnO2 film |