Research Article

Pulsed Eddy Current Nondestructive Testing for Defect Evaluation and Imaging of Automotive Lightweight Alloy Materials

Table 3

Minimum peak amplitude of defects in two directions.

Scanning directionDefect numberDefect 1Defect 2Defect 4Defect 5

directionNo defect (mV)4057.74
Min. amplitude (mV)3849.23636.13705.63663.1
Pct. change−5.14%−10.39%−8.68%−9.73%

directionNo defect (mV)4043.544
Min. amplitude (mV)3645.93458.53499.33584.2
Pct. change−9.83%−14.47%−13.46%−11.36%