Effect of Laser Emission Parameters on Mechanical and Physical Properties of Cast Pure Titanium

Figure 10

Hardness depth profiles from cast surface for control specimens (grade 2: black solid line, grade 3: red solid line) and specimens laser-treated with two different pulse durations (10 ms and 1 ms) at a constant emission current (220 A) and a spot diameter (1.0 mm).