Evaluation of Salmon Adhesion on PET-Metal Interface by ATR, FT-IR, and Raman Spectroscopy
Figure 5
(a) Sample M1 of PET-coated ECCS plate showing zones of salmon muscle adhesion; numbers indicate points of spectral analyses. (b) Layout of points for spectral analyses in urea-treated sample M2.