Research Article
Copper Incorporation into CdS Thin Films by Ionic Exchange in an Aqueous Solution Process at Room Temperature
Table 1
Cell parameters of CdS : Cu thin films obtained by XRD.
| Sample | a (Å) | c (Å) | Cell volume (Å3) | Crystallite size (nm) |
| L0 | 4.1053 | 6.6802 | 112.58 | 26.2 | L1 | 4.1053 | 6.6587 | 112.22 | 21.8 | L2 | 4.1053 | 6.6594 | 112.23 | 25.7 | L3 | 4.1053 | 6.6643 | 112.32 | 22.8 | L4 | 4.1053 | 6.6615 | 112.27 | 27.9 |
|
|