Research Article
Study on Crack Initiation and Propagation of New Corrosion Inhibitor during Stress Corrosion of Aluminum Alloy
Table 1
Fitting parameters of equivalent circuit.
| | Rs (Ω·cm2) | Rct (Ω·cm2) | Y0 (10−4Ω−1·cm−2·s−1) | ndl | ZCRACK (Ω·cm2) |
| Blank | 0.71–0.82 | 0.19–0.27 | 0.81–2.13 | 0.87–0.93 | 3284–3416 | Sodium succinate | 0.81–0.94 | 0.78–1.41 | 0.22–0.42 | 0.78–0.92 | 5150–5752 | New corrosion inhibitor | 0.69–0.79 | 0.21–0.38 | 0.8–2.31 | 0.76–0.95 | 4095–4271 | SDBS | 0.73–0.80 | 0.23–0.47 | 0.72–2.36 | 0.75–0.94 | 3386–3774 |
|
|