Research Article
Effect of Laser Heating on Partial Decomposition of Bi12SiO20 (BSO) Single Crystal: Raman Study
Figure 2
AFM results of: untreated Bi12SiO20 single crystal (a); laser treated Bi12SiO20 sample = 1.5 mW/μm2: 30 s (b); and 60 s (c).
(a) |
(b) |
(c) |