Dielectric Properties of Rhombohedral

Figure 10

Temperature dependent DC conductivity ( ) of the PbNb2O6 with rhombohedral phase, in the temperature range 400 to 700°C. Inset: temperature dependent relaxation time ( , in μs) of the same sample in the same temperature range.