Research Article
Durability Environmental Regionalization for Concrete Structures
Table 3
Detecting data of concrete structures (extract).
| Sample number | Durability environmental regionalization index | Concrete carbonation depth (mm) | Surface chloride concentration (%) | Ambient temperature (°C) | Ambient relative humidity (%) | Durability damage level |
| 1 | 17 | 1.39 | 23.91 | 80 | 3 | 2 | 27 | 0.80 | 23.25 | 72 | 1 | 3 | 18 | 2.18 | 23.5 | 79 | 3 | 4 | 16 | 1.59 | 23.94 | 83 | 4 | 5 | 9 | 1.98 | 23.31 | 85 | 4 | 6 | 22 | 0.80 | 23.25 | 75 | 2 | 7 | 20 | 2.18 | 23.67 | 80 | 3 | 8 | 28 | 0.01 | 22.46 | 74 | 2 | 9 | 26 | 0.20 | 22.59 | 72 | 1 | 10 | 17 | 2.78 | 23.28 | 79 | 3 | 11 | 25 | 0.39 | 22.32 | 74 | 2 | 12 | 7 | 2.18 | 23.17 | 86 | 4 | 13 | 12 | 2.97 | 23.88 | 84 | 4 | 14 | 16 | 1.19 | 22.66 | 84 | 4 | 15 | 21 | 0.60 | 23.12 | 78 | 3 | 16 | 26 | 0.99 | 22.47 | 73 | 2 | 17 | 21 | 2.58 | 22.9 | 80 | 3 | 18 | 10 | 2.18 | 23.55 | 85 | 4 | 19 | 22 | 0.99 | 22.41 | 80 | 3 | 20 | 10 | 2.38 | 22.74 | 86 | 4 | | 18.50 | 1.52 | 23.12 | 79.45 | 2.95 | | 6.26 | 0.88 | 0.51 | 4.76 | 0.97 |
|
|