Research Article
Data Mining of the Thermal Performance of Cool-Pipes in Massive Concrete via In Situ Monitoring
Table 2
Result of
(°C) output by the numerical model.
| (L/min) | (°C)
| 2.0 | 4.0 | 6.0 | 8.0 |
| 5 | 1.69 (2.28)* | 3.36 (4.43) | 5.11 (6.65) | 6.76 (8.41) | 10 | 1.58 (1.93) | 3.24 (3.82) | 4.41 (5.74) | 5.65 (7.25) | 20 | 1.17 (1.47) | 2.75 (2.93) | 3.36 (4.29) | 4.17 (5.30) | 30 | 0.86 (1.27) | 2.23 (2.44) | 2.90 (3.38) | 3.73 (3.99) | 40 | 0.79 (1.18) | 1.93 (2.15) | 2.83 (2.86) | 3.75 (3.23) | 50 | 0.80 (1.05) | 1.83 (1.87) | 2.81 (2.46) | 3.61 (2.77) | 60 | 0.79 (0.87) | 1.80 (1.50) | 2.64 (2.02) | 3.18 (2.38) | 70 | 0.87 (0.70) | 1.72 (1.12) | 2.29 (1.58) | 2.63 (2.03) | 80 | 1.02 (0.72) | 1.59 (0.93) | 1.91 (1.31) | 2.23 (1.81) | 90 | 1.01 (1.03) | 1.45 (1.08) | 1.78 (1.37) | 2.15 (1.84) | 100 | 0.76 (1.62) | 1.45 (1.58) | 2.03 (1.78) | 2.31 (2.16) |
|
|
*The number enclosed in brackets is the iron result, and the number outside of the brackets is the HDPE result.
|