Material thickness and material properties.

Sample typesLayersThickness
(m)
Conductivity
(W m−1 K−1)
Density
(kg m−3)

SJ0Clay bricks wall 0.2400.5081662

SJ1Recycled concrete bricks wall 0.240 0.7081887

SJ21 cement mortar 0.020 0.930 [16]1990
2 EPS insulation board 0.060 0.042 [16]29.50
3 recycled concrete bricks wall 0.2400.708 1887

SJ31 recycled concrete bricks wall 0.1150.7081887
2 cement mortar 0.0100.930 [16]1990
3 EPS insulation board 0.060 0.042 [16]29.50
4 cement mortar 0.0100.930 [16]1990
5 recycled concrete bricks wall 0.1150.7081887