| (%) | 2.5 | 9 | 15 | 20 | 25 | 30 |
| Sample nomenclature | 0 times | 1-0 | 2-0 | 3-0 | 4-0 | 5-0 | 6-0 | 1 time | 1-1 | 2-1 | 3-1 | 4-1 | 5-1 | 6-1 | 2 times | 1-2 | 2-2 | 3-2 | 4-2 | 5-2 | 6-2 | 3 times | 1-3 | 2-3 | 3-3 | 4-3 | 5-3 | 6-3 | 6 times | 1-4 | 2-4 | 3-4 | 4-4 | 5-4 | 6-4 | 9 times | 1-5 | 2-5 | 3-5 | 4-5 | 5-5 | 6-5 | 15 times | 1-6 | 2-6 | 3-6 | 4-6 | 5-6 | 6-6 |
|
|