Changes of mass fraction of caved gangue with different particle sizes before and after the testing.

Particle sizeMass fraction (%)
DryWater-saturated
Before testingAfter testingD-valueBefore testingAfter testingD-value

0–505.255.2505.855.85
5–1057.462.4658.093.09
10–151010.210.211010.430.43
15–202020.080.082020.250.25
20–253026.81-3.193026.68-3.32
25–302016.35-3.652015.05-4.95
30–35109.02-0.98108.86-1.14
35–4054.82-0.1854.78-0.22